** PLEASE CONTACT FOR PALLET PRICES.** PRODUCT INFORMATION ; DESCRIPTION: FGN 1300 is a cement-based, high-performance, hydraulic-binder joint grout. AREAS OF USE •Indoors and outdoors, •It is also used in the joint intervals of horizontally or vertically applied tiles, ceramics, etc. flooring. PRODUCT FEATURES AND ADVANTAGES •It becomes ready for use when mixed with water, •It is for joints between 0-6 mm, •Crack-free hardening, •Excellent adhesion, •Easy and smooth to use, •Provides a smooth surface. TECHNICAL SPECIFICATIONS Standard met: TS EN 13888 – CG1 Material composition: Contains special cements, polymers and mineral fillers. Color: White and Gray Compressive strength (EN 12808-3): ≥15 N/mm² Compressive strength after freeze-thaw cycles (EN 12808-3): ≥15 N/mm² Flexural strength (EN 12808-3): ≥3.5 N/mm² Flexural strength after freeze-thaw cycles (EN 12808-3): ≥3.5 N/mm² Shrinkage (EN 12808-4): ≤2 mm/m Abrasion resistance (EN 12808-2): ≤2000 mm³ Water Absorption 30 min. ≤5 g Water Absorption 240 min. ≤ 10 g (EN 12808): Temperature resistance: (-20°C) – (+70°C) Typical values: obtained as a result of experiments conducted on 4x4x16 cm mortar prisms at +23°C and 50% relative humidity conditions. High temperatures shorten the durations, low temperatures prolong them. APPLICATION METHOD Surface Preparation: Ensure that the tiles to be applied are thoroughly adhered and that the adhesive mortar has cured. Remove any dry mortar residues remaining in the joint gaps. Do not begin application without thoroughly cleaning all kinds of dust, cement residue, dirt, oil, etc. Make sure that the joint gaps are 2/3 of the tile thickness. Dampen the cleaned joint gaps before application. Pour a portion of the specified amount of water into a clean container. FGN 1300 is added slowly and mixed for 4 minutes with a 400-600 rpm mixer until a homogeneous and lump-free mixture is obtained. After allowing it to slake for approximately 4 minutes and mixing again for another 2 minutes, the material is ready for use. The mortar in the container should be consumed within approximately 1 hour depending on the ambient temperature. APPLICATION: The prepared mortar should be poured into the joint gaps and filled into the joints using a squeegee or a hard rubber-based grout spreader. Excess mortar remaining on the surface should be scraped off with a soft-tipped spatula. Depending on the ambient temperature, after 15-30 min., the thin grout film remaining on the application surface should be wiped with a damp sponge. The cleaning sponge must be cleaned frequently. Do not start the wiping process prematurely! MIXING RATIOS FOR 1 KG OF FGN 1300 FOR 20 KG BAG MIXING WATER AMOUNT: 0.3 lt – 0.35 lt 6 lt – 7 lt MIXING DENSITY: 1.45 kg/lt PACKAGING: 20 kg kraft bag. Also in 1 kg – 2 kg – 5 kg packages CONSUMPTION: For consumption, see the grout consumption table. SHELF LIFE: 12 months from the production date under suitable storage conditions. Opened packages must be stored under suitable storage conditions and used within one week.
Your orders are shipped within 1-3 business days. Shipping is free on orders of 500 ₺ and above. You can return the product within 14 days after receiving it.
Log in, you can write a review if you have purchased this product.
DESCRIPTION: TUĞ 1660 is a cement-based, high-performance, hydraulically hardening wide-joint grout developed specifically for decorative stone joints.